1、Adhesion and Damping in Skis RevisitedWorarin Meesron&Raphael SchallerCollano AG,Neulandstrasse 1,CH-6203 Sempach Station,Switzerland Adhesives&Bonding EXPO Europe,Messe Stuttgart GermanyDecember 5,2024OutlineBackgroundInspirationCase study:adhesionCase study:dampingOutlook3 Per Ivar SombyOlympic wi

2、nter games ad,St.Moritz,1948Howard Head,US Patent,2,995,379,1958Anavon,ski factory,2022BackgroundSki manufacturing process6Manual assemblySki pressBackgroundSki layout and materials7a)CoPA top sheetb)Aluminum top chordc)ABS sidewalld)Wood coree)Aluminum bottom chordf)Steel edgeg)UHMWPE running surfa

3、ceabcdefgCoPA:copolyamidABS:acrylonitrile-butadiene-styreneUHMWPE:ultra-high molecular weight polyethylene Epoxy used to bond the in dividual materialsIssueDelaminationFailure between aluminum and epoxy8Typical delamination failure in skisOutlineBackgroundInspirationCase study:adhesionCase study:dam

4、pingOutlook9InspirationMetal rear injection molding10Step 1:coatingStep 2:forming&stampingStep 3:rear injectionAdhesive filmCoated metal coilFormed metal sheetInsertInjection moldingEjectLaminating at elevated temperature&under pressure Metal coilInspirationMetal rear injection molding11 Novem Car I

5、nterior Design GmbHBMW X4 door lineMercedes-Benz S-Klasse instrument panelOutlineBackgroundInspirationCase study:adhesionCase study:dampingOutlook12Case study:adhesionFrom automotive to skis13Metal coilTPU/PE-film Coated metal coilTop&bottom chordManual assembly PressingT=170 Cp=1.5 barv=1 m/minDemo

6、ldingT=120 Cp=20 bart=20 minStep 1:coatingStep 2:shapingStep 3:ski makingTPU:thermoplastic polyurethanePE:polyethyleneCase study:adhesionTPU/PE-film coated aluminum14Peel resistance/N/mmDisplacement/mm Highest peel resistance with TPU/PE-filmInitial:aluminum used as delivered aluminum coated with TP

word格式文档无特别注明外均可编辑修改,预览文件经过压缩,下载原文更清晰!
三个皮匠报告文库所有资源均是客户上传分享,仅供网友学习交流,未经上传用户书面授权,请勿作商用。
本文主要探讨了滑雪板制造中的粘合和减震问题。关键点如下: 1. 粘合:采用金属后注射成型技术,以TPU/PE膜涂层的铝材粘合,经过气候测试后,其剥离阻力仍保持较高,使滑雪板铝材的粘合更可靠,降低了因分层导致的故障率从30%降至0%。 2. 减震:滑雪板中使用橡胶层减震。通过实验发现,含有Collano“Boost”和“React”粘合剂的滑雪板比使用橡胶层的标准滑雪板在减震性能上更受滑雪者好评。 核心数据: - 剥离阻力:TPU/PE膜涂层铝材表现出最高的剥离阻力。 - 弯曲振动:根据ISO 6267标准,含有Collano粘合剂的滑雪板在0°C时的弯曲振动位移小于标准橡胶层滑雪板。 - 应变率系数:Collano“Boost”和“React”产品的应变率系数高于标准橡胶层,表明其具有更好的应变率敏感性。 文章提出了两个未解决的问题:何为优质滑雪板?哪些实验室测量能预测滑雪板性能?
"滑雪板粘合新法怎样?" "如何大幅提升滑雪体验?" "新材料让滑雪板更稳定?"
客服
商务合作
小程序
服务号
折叠